7075 t6 aluminum plate

7075 t6 aluminum plate

  • 7075 aluminium alloy - Wikipedia

    OverviewMechanical propertiesBasic propertiesUsesTrade namesSee alsoFurther readingExternal links

    The mechanical properties of 7075 depend greatly on the tempering of the material. Un-heat-treated 7075 (7075-0 temper) has a maximum tensile strength of no more than 280 MPa (40,000 psi), and maximum yield strength of no more than 140 MPa (21,000 psi). The material has an elongation (stretch before ultimate failure) of 9–10%. As is the case for all 7075 aluminum alloys, 7075-0 is highly corrosion-resistant combined with generally acceptable strength profile.