Absolutely 5052-H32 for bending, unless you can tolerate *huge*bend radii (lest it crack), then 6061 or 2024 may be okay. 5052 3003 are the common alloys for
0.25′′ Aluminum 5052 Sheet Fabircation Sliver Painting Finish Bending, Find Details and Price about Bending Lock System Assembly from 0.25′′ Aluminum 5052 Sheet
Alloy 5052 is a non-heat-treatable 2.5% magnesium, 0.25% chromium alloy commonly available in flat rolled coil, sheet and plate from a wide range of producing mills. Like all